Chemical Composition
Silicon Si: 0.40
Iron Fe: 0.50
Copper Cu: 1.2-2.0
Manganese Mn: 0.30
Magnesium Mg: 2.1-2.9
Chromium Cr: 0.18-0.28
Zinc Zn: 5.1-6.1
Titanium Ti: 0.20
Aluminum Al: balance
Single: 0.05
Total: 0.15
Mechanical Property
Tensile strength 525Mpa
Yield strength 503Mpa
Elongation 11%
Hardness 150HB
Thickness 1-500mm
Appilcation
It is used to manufacture aircraft structures and other high-stress structural parts that require high strength and high corrosion resistance, such as aircraft upper and lower wing panels, purlins, and partitions. After solution treatment, the plasticity is good, the heat treatment strengthening effect is particularly good, the strength is below 150 ° C, and the low temperature strength is particularly good, the welding performance is poor, the stress corrosion cracking tendency is tendency, and the double-stage aging can improve the anti-SCC performance.
7075 sheet spot specification: 0.3mm-350mm (thickness)
7075 bars stock specification: 3.0mm-550mm (diameter)
7075 wires stock specification: 0.1mm-20mm (wires diameter)